Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 325 kJ/m² | 155 ft-lb/in² | ASTM D1822 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |