Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 325 kJ/m² | 155 ft-lb/in² | ASTM D1822 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Tensile Impact Strength | 326 kJ/m² @Temperature -40.0 °C |
155 ft-lb/in² @Temperature -40.0 °F |
ASTM D1822 |
ExxonMobil HD 6605.29 Injection Molding Resin
(discontinued **) HD 6605 is a narrow molecular weight hexene copolymer designed for a wide range of injection molding applications, offering excellent ESCR with good stiffness-toughness balance. Ideally suited for .. |