Polymer Property : Tensile Impact Strength = 30.9 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Impact Strength 65.0 - 160 kJ/m²
30.9 - 76.1 ft-lb/in²
Average value: 112 kJ/m² Grade Count:3
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim..
Tensile Impact Strength 65.0 kJ/m²
30.9 ft-lb/in²
LyondellBasell Lupolen® 6031 M HDPE, Injection Molding Grade
Easy flow, injection molding grade for fruit crates, tote boxes and bottle crates, cartridges, protective headgear, buckets, dishes, cartridges for adhesive film canisters, aerosol lids, child seats..