Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 65.0 - 160 kJ/m² | 30.9 - 76.1 ft-lb/in² | Average value: 112 kJ/m² Grade Count:3 |
Overview of materials for Polybutylene Terephthalate (PBT), Unreinforced, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Unreinforced, Molded". Each property range of values reported is minim.. |