Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 63.0 kJ/m² | 30.0 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 3412R PC (Asia Pacific) 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Tensile Impact Strength | 63.0 kJ/m² | 30.0 ft-lb/in² | Type S; ASTM D1822 |
Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced Form: PelletsInformation provided by Chase Plastics. |
|||
Tensile Impact Strength | 63.0 kJ/m² | 30.0 ft-lb/in² | Molded and tested in accordance with ASTM D4976; ASTM D1822, Type S |
Dow DMDA-8965 NT 7 High Density Polyethylene Resin DOW DMDA-8965 NT 7 is produced using UNIPOL™ process technology. It is intended for use in thin wall injection molding applications such as food containers. Information provided by Dow |
|||
Tensile Impact Strength | 63.0 kJ/m² | 30.0 ft-lb/in² | Type S; ASTM D1822 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |