Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Copolymer, 20% Glass Fiber Reinforced
Manufacturer Chase Plastics
Trade Name CP Pryme®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Chase Plastics CP Pryme® AH120 Acetal Copolymer, 20% Glass Fiber Reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Form: PelletsInformation provided by Chase Plastics.
Physical Properties Metric English Comments
Density 1.56 g/cc
0.0564 lb/in³
ASTM D792
Filler Content 20 %
20 %
Water Absorption 0.24 %
0.24 %
At 24 hrs; ASTM D570
Mechanical Properties Metric English Comments
Hardness, Rockwell M 89
89
ASTM D785
Tensile Strength at Break 56.5 MPa
8200 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Strength 70.3 MPa
10200 psi
ASTM D790
Flexural Modulus 5.17 GPa
750 ksi
ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
0.125 in; ASTM D256
Tensile Impact Strength 63.0 kJ/m²
30.0 ft-lb/in²
Type S; ASTM D1822
Thermal Properties Metric English Comments
Melting Point 173 °C
344 °F
Deflection Temperature at 0.46 MPa (66 psi) 176 °C
348 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 159 °C
318 °F
Unannealed; ASTM D648