Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 3.80 kJ/m² | 1.81 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LD-613 EVA Injection Molding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.An 8.8% vinyl acetate copolymer resin designed for molding and extrusion applications requiring low temperatures, flexibility and toughness. This r.. |