Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 530 kJ/m² | 252 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escor® AT-310 EMAAA Terpolymer for Polymer Modification
(discontinued **) Data provided by the manufacturer, Exxon Chemical.45 Acid Number. Provides unusual adhesion to a variety of substrates and other components such as aluminum foil, polyolefins, polycarbonate, PET, e.. |