Mechanical Properties Metric English Comments
Tensile Impact Strength 52.5 kJ/m²
25.0 ft-lb/in²
ASTM D1822
ExxonMobil Paxon™ BA7718 Sheet Extrusion and Blow Molding Resin  (discontinued **)
BA7718 is a 25% brown mica-filled, medium molecular weight, high density polyethylene. This material has been specifically developed as a cost effective resin for applications which require outstan..