Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Impact Strength | 231 kJ/m² | 110 ft-lb/in² | 23°C; ASTM D-1822 |
ExxonMobil Escorene® LL-5002 LLDPE Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A linear low density polyethylene resin designed to provide good processability and ease of blending. LL-5002 also exhibits good toughness and envi.. |
|||
Tensile Impact Strength | 231 kJ/m² | 110 ft-lb/in² | ASTM D1822 |
ExxonMobil HDPE AA48-002 High Density Polyethylene Resin Product Description: AA48-002 is a blow molding grade high density polyethylene copolymer containing an antistatic additive. It provides a very good balance of stress crack resistance, stiffness and.. |
|||
Tensile Impact Strength | 231 kJ/m² | 110 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AA45-004 Blow Molding Resin Product Description: AA45-004 is a blow molding high density polyethylene copolymer offering exceptional stress cracking resistance and impact performance.Availability: Latin America, North America .. |
|||
Tensile Impact Strength | 231 kJ/m² | 110 ft-lb/in² | ASTM D1822 |
ExxonMobil Paxon™ AG45-004 Blow Molding Resin
(discontinued **) AG45-004 is a blow molding high density polyethylene which offers exceptional stress crack resistance and impact performance. It contains an antistat which permits this resin to be used in all food.. |