ExxonMobil Paxon™ AA45-004 Blow Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Blow Molding Grade
Manufacturer Exxon Chemical
Trade Name Paxon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Paxon™ AA45-004 Blow Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: AA45-004 is a blow molding high density polyethylene copolymer offering exceptional stress cracking resistance and impact performance.Availability: Latin America, North America and South America Additive: Thermal Stabilizer: YesAntistatic: No Applications: Agricultural ProductsFood packagingHousehold and Industrial chemical containersPharmaceutical Packaging Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.945 g/cc
0.0341 lb/in³
ASTM D4883
ESCR 100% Igepal® >= 1000 hour
>= 1000 hour
ASTM D1693
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 24.1 MPa
3500 psi
ASTM D638
Elongation at Break 900 %
900 %
ASTM D638
Flexural Modulus 1.03 GPa
150 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
Tensile Impact Strength 231 kJ/m²
110 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Vicat Softening Point 121 °C
250 °F
ASTM D1525
Brittleness Temperature <= -76.1 °C
<= -105 °F
ASTM D746
Processing Properties Metric English Comments
Melt Temperature 191 °C
375 °F