Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0260 GPa | 3.77 ksi | ISO 37 |
Lubrizol ESTANE® GP72DB Ester Based Thermoplastic Polyurethane Type: Estane® GP 72DB is an aromatic polyester-based thermoplastic polyurethane (TPU).Appearance: Translucent spherical pelletsUses: Injection molding parts, TranslucentAvailable in EuropeInformati.. |
|||
100% Modulus | 0.0260 GPa | 3.77 ksi | ASTM D412 |
Wanhua Chemical Wanthane® WHT-1164 Polyester Based TPU Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd. |