Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Wanhua Chemical Wanthane® WHT-1164 Polyester Based TPU

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane TPE , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyester Grade
Manufacturer Wanhua Chemical Group Co., Ltd.
Trade Name Wanthane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Wanhua Chemical Wanthane® WHT-1164 Polyester Based TPU.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent mechanical properties, high abrasion resistance, tear resistance, short cycle timeInformation provided by Wanhua Chemical Group Co., Ltd.
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore D 72
72
ASTM D2240
Tensile Strength 42.0 MPa
6090 psi
ASTM D412
Elongation at Break 370 %
370 %
ASTM D412
100% Modulus 0.0260 GPa
3.77 ksi
ASTM D412
300% Modulus 0.0360 GPa
5.22 ksi
ASTM D412
Tear Strength 193 kN/m
1100 pli
ASTM D624
Abrasion 45
45
Abrasion resistance, mm<sup>3</sup>; ISO 4649
Processing Properties Metric English Comments
Processing Temperature 200 - 220 °C
392 - 428 °F