Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0197 GPa | 2.85 ksi | ASTM D-638 |
Axiall 15643 Wire & Cable Flexible PVC Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C. The compound is also formulated for fungus and microbe resistanc.. |
|||
100% Modulus | 0.0197 GPa | 2.85 ksi | ASTM D-638 |
Axiall 22561 Coax & Telecom Flexible PVC Non-lead stabilized, semi-rigid insulation compound for minimum transmission interference in communication applications. Suitable for use as a riser insulation.Information provided by Georgia GulfG.. |