Mechanical Properties Metric English Comments
100% Modulus 0.0197 GPa
2.85 ksi
ASTM D-638
Axiall 15643 Wire & Cable Flexible PVC
Non-lead stabilized semi-rigid insulation compound recommended for Style #1061 applications. Maximum service temperature of 105°C. The compound is also formulated for fungus and microbe resistanc..
100% Modulus 0.0197 GPa
2.85 ksi
ASTM D-638
Axiall 22561 Coax & Telecom Flexible PVC
Non-lead stabilized, semi-rigid insulation compound for minimum transmission interference in communication applications. Suitable for use as a riser insulation.Information provided by Georgia GulfG..