Mechanical Properties Metric English Comments
100% Modulus 0.0193 GPa
2.80 ksi
ASTM D412
SK Chemicals SKYTHANE® R155D Polyether Based Thermoplastic Polyurethane Elastomer
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets ..
100% Modulus 0.0193 GPa
2.80 ksi
ASTM D412
Lubrizol ESTANE® ETE55DT3 Ester Based Thermoplastic Polyurethane
Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, UV stableUses: Extrusion: Hose and Tube, Extrusion: Profile, Cable Jacket..
100% Modulus 0.0193 GPa
2.80 ksi
ASTM D412
Lubrizol Estane® 2103-65D Thermoplastic Polyurethane Elastomer
Formerly PellethaneFeature: Low temperature impactAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in..
100% Modulus 0.0193 GPa
2.80 ksi
ASTM D-638
Axiall 14630 Wire & Cable Flexible PVC
Semi-rigid, flame retardant jacketing compound recommended. Also suitable for semi-rigid molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0193 GPa
2.80 ksi
ASTM D-638
Axiall 21571 Coax & Telecom Flexible PVC
Semi-rigid insulation compound designed for data communication riser cable application.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0193 GPa
2.80 ksi
Dow Pellethane® 2354-65D Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2354-65D elastomer is a polyester polycaprolactone based polyurethane elastomer used in automotive applications. It allows fast molding, and once molded can be painted with polyurethane..