Polymer Property : 100% Modulus = 2.65 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0183 GPa
2.65 ksi
ASTM D-638
Axiall 19471 Wire & Cable Flexible PVC
Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia ..