Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0183 GPa | 2.65 ksi | ASTM D-638 |
Axiall 19471 Wire & Cable Flexible PVC Semi-rigid, 105°C insulation compound recommended for a minimum wall thickness of 10 mils. Designed to meet the performance criteria of military spec. MIL-W-16878D.Information provided by Georgia .. |