Mechanical Properties Metric English Comments
100% Modulus 0.0179 GPa
2.60 ksi
ASTM D412
Lubrizol Estane® ALR E65D Thermoplastic Polyurethane
Type: Estane® ALR E65D is a clear aliphatic thermoplastic polyurethane (TPU).Features: Non-yellowing with good mechanical properties.Available in AmericasInformation Provided by The Lubrizol Corpor..
100% Modulus 0.0179 GPa
2.60 ksi
ASTM D638
Colorite Polymers 9833 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.0179 GPa
2.60 ksi
ASTM D-638
Axiall 11470 Wire & Cable Flexible PVC
Highly flame retardant clear compound. Recommended as jacket in PVC/PVC VW-1 constructions.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.0179 GPa
2.60 ksi
ASTM D412/D638
Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane
Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability unde..
100% Modulus 0.0179 GPa
2.60 ksi
ASTM D-638
Axiall 4520 Flexible PVC
Non-lead stabilized, thin wall, 105C rated automotive harness compound.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.