Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 5778 Ester Based Thermoplastic Polyurethane.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features: It is especially well suited for dispersing co-ferrite as well as Cr02 pigments used in video, audio, and data storage applications. This product offers excellent hydrolytic stability under accelerated test conditions as well as outstanding pigment dispersion characteristics. Because of its medium Tg, it offers excellent adhesion and easier calendaring for high quality video and audio formulations. An excellent video tape can be formulated by blending with other harder dispersing resins. It is also used for dispersing high-surface–area pigments as a polymeric dispersant.Uses: Tape binder, inks, lacquers and polymeric dispersing polymer for pigment dispersionAvailable in Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol.
Physical Properties Metric English Comments
Specific Gravity 1.21 g/cc
1.21 g/cc
ASTM D792
Brookfield Viscosity 60 - 70 cP
60 - 70 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in MEK
70 - 80 cP
70 - 80 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in THF
180 - 200 cP
180 - 200 cP
RVT Spindle #2, 20 RPM, 23°C, 15% T.S. in Cyclohexanone
Mechanical Properties Metric English Comments
Hardness, Shore D 78
78
ASTM D224
Tensile Strength 34.5 MPa
5000 psi
ASTM D412/D638
Elongation at Break 250 %
250 %
ASTM D412/D638
100% Modulus 0.0179 GPa
2.60 ksi
ASTM D412/D638
Thermal Properties Metric English Comments
Vicat Softening Point 37.8 °C
100 °F
ASTM D1525
Glass Transition Temp, Tg 31.0 °C
87.8 °F
DSC