Mechanical Properties Metric English Comments
100% Modulus 0.01410 GPa
2.045 ksi
Plasticizer conc. in vinyl film 40 phr; ASTM D638
BASF Palatinol® N Diisononyl Phthalate
Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl..