Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0127 GPa | 1.84 ksi | |
Taiwan PU Corporation TPUI-E98 General Grade, Injection Molding Polyester Base TPU Thermoplastic Polyurethane (TPU), General Grade, Polyester Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.0127 GPa | 1.84 ksi | |
Taiwan PU Corporation TPUI-G98 High Wear Resistance, Injection Molding Polycaprolactone Base TPU Thermoplastic Polyurethane (TPU), High Wear Resistance, Polycaprolactone Base, Injection MoldingInformation provided by Taiwan PU Corporation. |
|||
100% Modulus | 0.0127 GPa | 1.84 ksi | EVA/NBR Strippable Compounds |
TIMCAL ENSACO™ 250G Conductive Carbon Black ENSACO™ & SUPER P™ conductive carbon blacks are carbon blacks with a high to very high void volume allowing the retention of a carbon network at low to very low filler content. The void volume can.. |