Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.01202 GPa | 1.743 ksi | ASTM D412 |
Lubrizol Advanced Materials PEARLTHANE® 11H94 Thermoplastic Polyurethane Elastomer PEARLTHANE® D11H94 is a high performance polycaprolactone copolyester based TPU, supplied in form of translucent, colorless pellets, featuring adequate hardness as well as excellent flow and mech.. |