Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00860 GPa | 1.25 ksi | DIN 53504 |
Lubrizol ESTANE® T4057 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D412 |
Teknor Apex UNIPRENE® 7010-40D Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
100% Modulus | 0.00860 GPa | 1.25 ksi | DIN 53504 |
Lubrizol ESTANE® 58092 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D638 |
Colorite Polymers 8088 Non-Phthalate 88 Series Vinyl Compound Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo.. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D-638 |
Axiall 18770 Moldings & Extrusions Flexible PVC General purpose 105C, clear jacketing compound recommended for 1/32" wall and larger. Exhibits excellent migration properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat.. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D-638 |
Axiall 8801 Moldings & Extrusions Flexible PVC General purpose clear extrusion compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D-638 |
Axiall 19840 Wire & Cable Flexible PVC 105°C rated insulation suitable for 1/64 wall. Recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D638 |
Colorite Polymers 8000 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00862 GPa | 1.25 ksi | ASTM D638 |
Colorite Polymers 8002 General Purpose Vinyl Compound Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r.. |
|||
100% Modulus | 0.00860 GPa | 1.25 ksi | TPE-0153 (ASTM D 412) |
Advanced Elastomer Systems Santoprene® 283-40 Thermoplastic Rubber
(discontinued **) A colorable thermoplastic medical grade elastomer with good fluid resistance, certified non-toxic by MEM elution test. It has USP Class VI Certificate of Compliance for biocompatibility and can be .. |
|||
100% Modulus | 0.00860 GPa | 1.25 ksi | ASTM D412 |
Lubrizol ESTANE® 58211 Ether Based Thermoplastic Polyurethane Features: Halogenated flame retardant compound – High hardnessUses: Extrusion – wire and cable jacketing and general extrusion where flame retardant propertied are requiredAvailable in Americas, E.. |