Mechanical Properties Metric English Comments
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D412
Teknor Apex UNIPRENE® 7010-40D Thermoplastic Elastomer
Information provided by Teknor Apex Company
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D638
Colorite Polymers 8088 Non-Phthalate 88 Series Vinyl Compound
Description: The Colorite 88 series is a family of vinyl non-toxic compounds formulated to provide excellent low temperature flexibility characteristics. These compounds are designed for outside doo..
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D-638
Axiall 18770 Moldings & Extrusions Flexible PVC
General purpose 105C, clear jacketing compound recommended for 1/32" wall and larger. Exhibits excellent migration properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporat..
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D-638
Axiall 8801 Moldings & Extrusions Flexible PVC
General purpose clear extrusion compound with good low temperature properties.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D-638
Axiall 19840 Wire & Cable Flexible PVC
105°C rated insulation suitable for 1/64 wall. Recommended for AWM applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D638
Colorite Polymers 8000 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00862 GPa
1.25 ksi
ASTM D638
Colorite Polymers 8002 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..