Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 100% Modulus = 1.09 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00750 GPa
1.09 ksi
Injection molded parts; DIN 53504
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester
Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN ..
100% Modulus 0.00752 GPa
1.09 ksi
Spartech E65090 General Purpose PVC
First choice for compounds meeting the stringent requirements of Spiral Hose, Automotive, Housewares, Farm Equipment, Coated Fencing and numerous other applications including Lawn & Garden Wheels. B..
100% Modulus 0.00750 GPa
1.09 ksi
ASTM D412 (Dumbbells)
DuPont Performance Polymers Kalrez® 8085 Gas Deposition Compound
Kalrez® Sahara™ 8085 is a new, specialty compound specifically developed for gas deposition applications, i.e., HDPCVD, PECVD, SACVD, etc. It has been specifically formulated for minimal particle ..
100% Modulus 0.00752 GPa
1.09 ksi
ASTM D638
Colorite Polymers 6476 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00750 GPa
1.09 ksi
ASTM D412
C.O.I.M. LARIPUR® LPR9060EM PTMG Polyether Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
100% Modulus 0.00750 GPa
1.09 ksi
ISO 37
AlphaGary Evoprene™ 057 Standard SBS Thermoplastic Elastomer Compound
The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han..
100% Modulus 0.00750 GPa
1.09 ksi
ISO 37
Termopol Termoton® K2GA4055D TPE Compound, based on SEBS and Polyolefins
Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t..
100% Modulus 0.00752 GPa
1.09 ksi
ASTM D-638
Axiall 38602 Coax & Telecom Flexible PVC
CATV and general purpose jacket with excellent low temperature properties. UL recognized for 720 hour sunlight resistance in all colors.Information provided by Georgia GulfGeorgia Gulf became Axial..
Copyright © lookpolymers.com All Rights Reserved