Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00750 GPa | 1.09 ksi | Injection molded parts; DIN 53504 |
Huntsman IROGRAN® A 92 E 4860 TPU-Polyester Introduction: IROGRAN A92E 4860 is a high performance polyester based thermoplastic polyurethane intended for extrusion and injection molding applications. IROGRAN A92E 4860 is part of the HUNTSMAN .. |
|||
100% Modulus | 0.00750 GPa | 1.09 ksi | ASTM D412 (Dumbbells) |
DuPont Performance Polymers Kalrez® 8085 Gas Deposition Compound Kalrez® Sahara™ 8085 is a new, specialty compound specifically developed for gas deposition applications, i.e., HDPCVD, PECVD, SACVD, etc. It has been specifically formulated for minimal particle .. |
|||
100% Modulus | 0.00750 GPa | 1.09 ksi | ASTM D412 |
C.O.I.M. LARIPUR® LPR9060EM PTMG Polyether Polyurethane Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion.. |
|||
100% Modulus | 0.00750 GPa | 1.09 ksi | ISO 37 |
AlphaGary Evoprene™ 057 Standard SBS Thermoplastic Elastomer Compound The Evoprene™ Standard is a styrene-butadiene -styrene based thermoplastic elastomer.Applications: extruded door, window and furniture seals and rubbing strips, mats, bump stops, grommets, coat han.. |
|||
100% Modulus | 0.00750 GPa | 1.09 ksi | ISO 37 |
Termopol Termoton® K2GA4055D TPE Compound, based on SEBS and Polyolefins Main Characteristics: Wide range of hardness; High strength elasticity; 100% recyclable; Easy processing by means of the traditional technologies for thermoplastic materials; Additional resistance t.. |