Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.007412 GPa | 1.075 ksi | ASTM D-638 |
Axiall 10753 Wire & Cable Flexible PVC Flame retardant 60C compound suitable for integral non-metallic conduit and general purpose jacket applications. Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |