Polymer Property : 100% Modulus = 1.05 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00724 GPa
1.05 ksi
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based  (discontinued **)
PELLETHANE® 2102-85A elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced UV stability and good hydrolytic stab..
100% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00724 GPa
1.05 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FC 2174 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FC 2174 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul..
100% Modulus 0.00724 GPa
1.05 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FE 5640Q Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FE 5640Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu..
100% Modulus 0.00724 GPa
1.05 ksi
ASTM D-638
Axiall 10852 Wire & Cable Flexible PVC
General purpose non-lead stabilized jacket compound recommended for UL 75°C applications or 80C automotive applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in..
100% Modulus 0.00724 GPa
1.05 ksi
ASTM D-638
Axiall 11800 Wire & Cable Flexible PVC
Designed for 75°C rated cords and cord sets and other general purpose insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00724 GPa
1.05 ksi
ASTM D-638
Axiall 17800 Wire & Cable Flexible PVC
Clear PVC compound best suited for 90C applications at 1/32" wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
100% Modulus 0.00724 GPa
1.05 ksi
ASTM D-638
Axiall 18730 Wire & Cable Flexible PVC
UL recognized 720 hour sunlight resistant in all colors, oil resistant, 105 C rated PVC jacket compound with good low temperature performance. Information provided by Georgia GulfGeorgia Gulf became..
100% Modulus 0.00724 GPa
1.05 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N220 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00724 GPa
1.05 ksi
DuPont Performance Polymers Kalrez® 6221 FFKM Perfluoroelastomer
Kalrez® parts made from compounds 6221 provide superior chemical resistance and low contamination from extractables in pharmaceutical and food handling applications where FDA compliance is required..