Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00724 GPa | 1.05 ksi | |
Dow Pellethane® 2102-85A Polyurethane Elastomer, Polyester Polycaprolactone Based
(discontinued **) PELLETHANE® 2102-85A elastomer is a polyester polycaprolactone based polyurethane elastomer which combines excellent resistance to fuels and oils with enhanced UV stability and good hydrolytic stab.. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FC 2174 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FC 2174 can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formul.. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FE 5640Q Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FE 5640Q can be compounded using standard water cooled internal mixers or two-roll mills with standard fillers and ingredients utilized in typical fluoroelastomer formu.. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | ASTM D-638 |
Axiall 10852 Wire & Cable Flexible PVC General purpose non-lead stabilized jacket compound recommended for UL 75°C applications or 80C automotive applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in.. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | ASTM D-638 |
Axiall 11800 Wire & Cable Flexible PVC Designed for 75°C rated cords and cord sets and other general purpose insulations.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | ASTM D-638 |
Axiall 17800 Wire & Cable Flexible PVC Clear PVC compound best suited for 90C applications at 1/32" wall and larger.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | ASTM D-638 |
Axiall 18730 Wire & Cable Flexible PVC UL recognized 720 hour sunlight resistant in all colors, oil resistant, 105 C rated PVC jacket compound with good low temperature performance. Information provided by Georgia GulfGeorgia Gulf became.. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | |
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR N220 Filler MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje.. |
|||
100% Modulus | 0.00724 GPa | 1.05 ksi | |
DuPont Performance Polymers Kalrez® 6221 FFKM Perfluoroelastomer Kalrez® parts made from compounds 6221 provide superior chemical resistance and low contamination from extractables in pharmaceutical and food handling applications where FDA compliance is required.. |