Polymer Property : 100% Modulus = 1.008 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.006950 GPa
1.008 ksi
Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C
3M Dyneon™ FG 5661 Fluoroelastomer
3M™ Dyneon™ Fluoroelastomer FG 5661 can be compounded using standard water cooled internal mixers or two-roll mills. The “dry” ingredients should be blended before adding to the masticated gum. ..