Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.006950 GPa | 1.008 ksi | Press Cure 5 minutes @ 177°C, Post Cure 24 hours @ 260°C |
3M Dyneon™ FG 5661 Fluoroelastomer 3M™ Dyneon™ Fluoroelastomer FG 5661 can be compounded using standard water cooled internal mixers or two-roll mills. The “dry” ingredients should be blended before adding to the masticated gum. .. |