Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00641 GPa | 0.930 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2090 BK Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |
|||
100% Modulus | 0.00641 GPa | 0.930 ksi | ASTM D412; ISO 37 |
Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod.. |