Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer APA - Advanced Polymer Alloys
Trade Name Alcryn®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Advanced Polymer Alloys Alcryn® 2090 NC Melt Processable Rubber.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high productivity on thermoplastic processing equipment.Applications:Window and door weatherstripping (and other complex profile extrusions)Soft handles and gripsMolded seals and gasketsInjection-molded and co-injection molded partsBlow-molded partsTubing and hoseWire and cable jacketsCoated fabrics and sheet goodsInformation provided by Advanced Polymer Alloys
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
ASTM D471; ISO 2781
Viscosity 550000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
550000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
ASTM D2240; ISO 48
Tensile Strength, Ultimate 0.255 MPa
37.0 psi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
10.8 MPa
1570 psi
ASTM D412; ISO 37
Elongation at Break 320 %
320 %
ASTM D412; ISO 37
100% Modulus 0.000490 GPa
0.0710 ksi
After 7 days at 257°F (125°C); ASTM D573; ISO 188
0.00641 GPa
0.930 ksi
ASTM D412; ISO 37
Compression Set 27 %
27 %
After 22 Hr at 75°F (24°C); ASTM D395; ISO 815
74 %

@Temperature 100 °C
74 %

@Temperature 212 °F
22 hrs.; ASTM D395; ISO 815
Tensile Set 13 %
13 %
ASTM D412
Thermal Properties Metric English Comments
Clash Berg Stiffness Temperature -5.00 °C
23.0 °F
At 10,000 psi (69 Mpa); ASTM D1043
Processing Properties Metric English Comments
Processing Temperature 177 °C
350 °F
Descriptive Properties Value Comments
Fluid Resistance - Volume Change, % (ASTM D471) -10
After 7 Days in ASTM Oil No.1 at 212°F (100°C)
-23
After 7 Days in IRM 903 Oil No.3 at 212°F (100°C)
36
After 7 Days in ASTM Ref. Fuel No. B at 75°F (24°C)