Polymer Property : 100% Modulus = 0.89883 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.0061971 GPa
0.89883 ksi
-31.9% change after 72 hours @ 250°C; ASTM D412
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer
A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app..