Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.0061971 GPa | 0.89883 ksi | -31.9% change after 72 hours @ 250°C; ASTM D412 |
Precision Polymer Engineering Perlast® G60A Perfluoroelastomer A black general purpose perfluoroelastomer compound with excellent chemical resistance, steam resistance and mechanical properties. Extremely low outgassing properties.Applications: Suitable for app.. |