Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00543 GPa | 0.788 ksi | Heat Age Resistance, 70 Hour @ 270°C |
3M Dyneon™ RA 5300 High Performance Rubber Additive 3M™ Dynamar™ RA 5300 High Performance Rubber Additive is designed for use at low loadings to improve the processing in extrusion and molding operations. It utilizes unique chemistry which makes it.. |