Polymer Property : 100% Modulus = 0.00543 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
100% Modulus 0.00543 GPa
0.788 ksi
Heat Age Resistance, 70 Hour @ 270°C
3M Dyneon™ RA 5300 High Performance Rubber Additive
3M™ Dynamar™ RA 5300 High Performance Rubber Additive is designed for use at low loadings to improve the processing in extrusion and molding operations. It utilizes unique chemistry which makes it..