Mechanical Properties Metric English Comments
100% Modulus 0.00451 GPa
0.654 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00451 GPa
0.654 ksi
ASTM D412
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film
Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta..
100% Modulus 0.00451 GPa
0.654 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..