Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00451 GPa | 0.654 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |
|||
100% Modulus | 0.00451 GPa | 0.654 ksi | ASTM D412 |
SK Chemicals SKYTHANE® UB400 Hotmelt Lamination Film Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
100% Modulus | 0.00451 GPa | 0.654 ksi | |
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, 3.0 PHR Luperco 130XL Peroxide Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m.. |