Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00392 GPa | 0.568 ksi | |
Taiwan Sheen Soon Sheenthane® A8000F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00392 GPa | 0.568 ksi | |
Taiwan Sheen Soon Sheenthane® A8210F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |