Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.00392 GPa | 0.568 ksi | |
Taiwan Sheen Soon Sheenthane® A8000F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00392 GPa | 0.568 ksi | |
Taiwan Sheen Soon Sheenthane® A8210F Thermoplastic Polyurethane Elastomer Thermoplastic polyurethane elastomer for extrusionInformation provided by Taiwan Sheen Soon Co., LTD. |
|||
100% Modulus | 0.00392 GPa | 0.569 ksi | JIS K6301 |
Stellarchem GP-930 TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
100% Modulus | 0.00392 GPa | 0.569 ksi | JIS K6301 |
Stellarchem HP-930NC-HD TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
100% Modulus | 0.00392 GPa | 0.569 ksi | JIS K6301 |
Stellarchem LP-830 TPE Compound This grade of Stellarchem LP series is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, styrene block copolymers based, .. |
|||
100% Modulus | 0.00392 GPa | 0.569 ksi | ASTM D638 |
SK Chemicals SKYTHANE® U0351C Ink Binder Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
100% Modulus | 0.00392 GPa | 0.569 ksi | JIS K6301 |
Stellarchem 475-845N TPE Compound This grade of Stellarchem TPE is shear dependent and can be processed on conventional thermoplastics equipment for injection molding or extrusion. It's a soft, elastomeric polyolefin based, complete.. |
|||
100% Modulus | 0.00392 GPa | 0.569 ksi | ASTM D412 |
SK Chemicals SKYTHANE® UB420 Hotmelt Lamination Film Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |