Mechanical Properties Metric English Comments
100% Modulus 0.00314 GPa
0.455 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00314 GPa
0.455 ksi
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane, 285ºF Cure Temperature
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
100% Modulus 0.00314 GPa
0.455 ksi
500 mm/min; ASTM D 412
Zylog Neoplast® 155 FT EB Thermoplastic Vulcanizate
Neoplast 155 FT EB is a soft, dynamically vulcanized thermoplastic vulcanizate (TPV), based on polyolefin chemistry, and is intended for Injection Molding and Extrusion applications.RoHS Compliant, ..
100% Modulus 0.00314 GPa
0.455 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..
100% Modulus 0.00314 GPa
0.455 ksi
TSE Industries Millathane® 76 Millable Polyester Polyurethane Rubber, Hardness 60A, Non-Black Sulfur Cure
Millathane® 76 is a very suitable choice for use in products such as bushings, small copier rolls; automotive applications — bumpers, o-rings, hydraulic seals, belts, gaskets, solid tires — and m..