Mechanical Properties Metric English Comments
100% Modulus 0.00293 GPa
0.425 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00293 GPa
0.425 ksi
Shin-Etsu Silicones SV-17500U Silicone Rubber
SV17500U is one of a series of easy processing, silicone rubber bases. It can be used in a variety of applications requiring finishing by molding, extruding or calendaring. Product Features: This pr..
100% Modulus 0.00293 GPa
0.425 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 30 PHR N330 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00293 GPa
0.425 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00293 GPa
0.425 ksi
ASTM D638
Colorite Polymers 6284 General Purpose Vinyl Compound
Description: Colorite produces many vinyl compounds. They have the compounds that perfectly suit whatever the application. Requirements such as ultraviolet ray resistance, fungus resistance, flame r..
100% Modulus 0.00293 GPa
0.425 ksi
ASTM D-638
Axiall 8552 Moldings & Extrusions Flexible PVC
A soft extrusion compound recommended for profiles, weatherstrips and sheeting. Also suitable for injection molding.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 201..
100% Modulus 0.00293 GPa
0.425 ksi
TSE Industries Millathane® CM Millable Polyether Urethane Rubber with 75 PHR Hi-Sil 233 Filler
MILLATHANE CM is a sulfur and peroxide curable polyether urethane rubber. Its outstanding property is its great resistance to abrasion, which makes it of special interest for articles that are subje..
100% Modulus 0.00293 GPa
0.425 ksi
ASTM D412
Saint-Gobain Tygon® 2375 Ultra Chemical Resistant Tubing Formulation
Tygon® Ultra Chemical Resistant Tubing offers a combination of chemical resistance, clarity and flexibility. Tygon® 2375 replaces 2075.Tygon® Ultra Chemical Resistant Tubing is virtually unaffec..