100% Modulus 0.02051 GPa
2.975 ksi
ASTM D-638
Axiall 15641 Wire & Cable Flexible PVC
Semi-rigid, fungus and microbe resistant insulation compound recommended for UL Style #1061 and CSA-SR applications. The compound has good migration and toner resistance.Information provided by Geo..