Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.01600 GPa | 2.320 ksi | ASTM D412 |
Lubrizol Advanced Materials Pearlthane® D91F65D Thermoplastic Polyurethane Elastomer PEARLTHANE® D91F65D is an aliphatic TPU supplied in colourless natural pellets. In addition to typical TPU properties like outstanding abrasion loss, PEARLTHANE® D91F65D offers excellent colou.. |