Mechanical Properties | Metric | English | Comments |
---|---|---|---|
100% Modulus | 0.01193 GPa | 1.730 ksi | ISO 37 |
PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer
(discontinued **) This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color.. |