Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer  (discontinued **)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Elastamax XL-0257-2 TPU-Based Thermoplastic Elastomer  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a general purpose thermoplastic elastomer based on TPU for injection molding, and has a high specific gravity for applications requiring high weight. Physical Form: Pellets. Standard Color: Grey.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.
Physical Properties Metric English Comments
Melt Flow 212 g/10 min

@Load 2.16 kg,
Temperature 210 °C
212 g/10 min

@Load 4.76 lb,
Temperature 410 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 51
51
5 sec. delay; ASTM D2240
Tensile Strength, Ultimate 15.9 MPa
2310 psi
10 in/min; ASTM D412
Elongation at Break 212 %
212 %
10 in/min; ASTM D412
50% Modulus 0.01145 GPa
1.661 ksi
10 in/min; ASTM D412
100% Modulus 0.01193 GPa
1.730 ksi
ISO 37
Izod Impact, Notched 3.74 J/cm

@Thickness 3.17 mm
7.01 ft-lb/in

@Thickness 0.125 in
ASTM D256
Copyright © lookpolymers.com All Rights Reserved