Polymer Property : 100% Modulus = 0.00914 GPa
Polymer Property :
100% Modulus =
0.00914 GPa
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
100% Modulus
0.00914
GPa
1.33
ksi
C.O.I.M. PLAXTER® P 05 Low Viscosity Polymeric Plasticizer
Description: Used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc.