C.O.I.M. PLAXTER® P 05 Low Viscosity Polymeric Plasticizer

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic
Manufacturer C.O.I.M. S.p.A.
Trade Name PLAXTER®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF C.O.I.M. PLAXTER® P 05 Low Viscosity Polymeric Plasticizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Used in the field of adhesive tapes.Information provided by P.A.T. Products, Inc.
Physical Properties Metric English Comments
Viscosity 800 - 1200 cP

@Temperature 35.0 °C
800 - 1200 cP

@Temperature 95.0 °F
Dynamic viscosity
Mechanical Properties Metric English Comments
Hardness, Shore D 71
71
Tensile Strength, Yield 27.8 MPa
4030 psi
Elongation at Break 260 %
260 %
100% Modulus 0.00914 GPa
1.33 ksi
Optical Properties Metric English Comments
Gardner Color Number 2.0
2.0
Chemical Properties Metric English Comments
Acid Value 2.0
2.0
mgKOH/g
Descriptive Properties Value Comments
Efficiency concentration PHR 33.5
N OH value (max) 20
mg KOH/g